CLEANING MATERIAL COVERING MEMBER, ITS PRODUCTION METHOD AND PRODUCTION METHOD FOR CLEANING MATERIAL COVERING YARN |
摘要 |
<P>PROBLEM TO BE SOLVED: To provide a cleaning material covering member having high performance and covered with a photocatalyst or the like at low cost. <P>SOLUTION: The cleaning material covering member has a substrate (11); and a covering layer (12) comprising particulate apatite-covered titanium dioxide stuck onto a surface of the substrate without a mixing binder. Since the mixing binder is not used, the cleaning material covering member having high performance is obtained with sufficient productivity at low cost. <P>COPYRIGHT: (C)2005,JPO&NCIPI |