摘要 |
PROBLEM TO BE SOLVED: To provide a glass substrate having high resistance to thermal shock without being tempered; and to obtain a glass composition. SOLUTION: The glass composition contains glass components of 45-75 wt.% (hereinafter expressed as %) SiO<SB>2</SB>, 1-20% Al<SB>2</SB>O<SB>3</SB>, 0-8% B<SB>2</SB>O<SB>3</SB>, 60-90% of SiO<SB>2</SB>+ Al<SB>2</SB>O<SB>3</SB>+ B<SB>2</SB>O<SB>3</SB>, 0-20%, in total, of R<SB>2</SB>O (R = Li, Na and K), 0-20%, in total, of R'O (R' = Mg, Ca, Sr, Ba and Zn), and 0-12% of TiO<SB>2</SB>+ ZrO<SB>2</SB>+ Ln<SB>x</SB>O<SB>y</SB>(wherein, Ln<SB>x</SB>O<SB>y</SB>means at least one compound selected from the group of lanthanoid metal oxides, Y<SB>2</SB>O<SB>3</SB>, Nb<SB>2</SB>O<SB>5</SB>, and Ta<SB>2</SB>O<SB>5</SB>). COPYRIGHT: (C)2005,JPO&NCIPI
|