摘要 |
<p><P>PROBLEM TO BE SOLVED: To effectively use a low grade collected aromatic polycarbonate resin and a low grade collected styrenic resin each having deteriorated physical properties and contaminated with foreign matters to provide an injection molded article having added values comprising excellent characteristics such as excellent flame retardance, rigidities, impact resistance, appearances and flowability. <P>SOLUTION: The recycled aromatic polycarbonate resin composition is characterized by comprising (A) 50 to 80 wt.% of an aromatic polycarbonate resin, (B) 5 to 20 wt.% of a styrenic resin, (C) 0 to 20 wt.% of a halogen-free phosphate, and (D) 3 to 10 wt.% of a core-shell type graft rubbery elastomer, wherein at least one part of the component (A) and/or the component (B) is obtained by removing≥0.2 mm<SP>2</SP>foreign matters from the crushed products of the collected aromatic polycarbonate resin and/or the collected styrenic resin. The injection molded article is obtained from the recycled aromatic polycarbonate resin composition. <P>COPYRIGHT: (C)2005,JPO&NCIPI</p> |