发明名称 METHOD FOR PRODUCING OF ADDITION ALLOY FOR STEEL DEOXIDATION
摘要 FIELD: metallurgy and foundry. ^ SUBSTANCE: method includes mixing of aluminum and titanium powders with followed pressure. Additionally in powder composition iron powder is introduced. Composition contains (mass %): aluminum 4-38, titanium 6-60 and balance: iron. Pressure is carried out at 2000-25000 kg/cm2; powders are manufactured from chip produced as waste product. ^ EFFECT: reduced steel contamination by alumina, being capable of degrading of steel mechanical properties and workability. ^ 1 tbl, 3 ex
申请公布号 RU2241059(C1) 申请公布日期 2004.11.27
申请号 RU20030105598 申请日期 2003.02.26
申请人 发明人 TIMOFEEV G.I.;CHEBERJAK O.I.;JANBAEV F.M.;KOLPAKOV A.A.;MATVEICHEV S.I.;MITENKOVA L.P.
分类号 C22C35/00;C22C1/04 主分类号 C22C35/00