Cracking site for fracture separation of thermoplastic objects |
摘要 |
The line of intentional breakage is obtained by stages of partial mold filling, their extent being defined by the edge profile of a sliding core (3), which coincides with a weakened zone of reduced cross section. The line of weakness is obtained by coincidence of the zone weakened by a thinned section, and fusion between different parts of the molding. The molding flow lines do not cross the weakened zone having a reduced cross section.
|