FIELD: rocket fuels. ^ SUBSTANCE: method comprises formation of charge at temperature of fuel body by 10-20 below curing temperature and curing under pressure. Press mold, prior to be filled, is heated for 0.5 to 12 h at temperature by 5-10 superior to molding temperature and charge is then formed in press mold heated with air supplied under casing or flexible jacket of press mold at temperature by 10 superior to molding temperature. ^ EFFECT: improved quality of charge regarding its solidity and equilibrium temperature, and excluded undesired pressure surge during curing. ^ 2 dwg, 1 tbl |