发明名称 Method for manufacturing fuel inlet
摘要 In manufacturing a fuel inlet, bulge forming and bend processing are conducted to a stainless pipe which will serve as an inlet pipe. Next, one end of the stainless pipe is eccentrically expanded, and the hardened portion is removed. After the pipe expanding step is finished, boring processing is conducted so that a breather pipe can be inserted into the inlet pipe, a guide is spot-welded to the inside of the eccentrically expanded portion, and a screw structure is formed. The inlet pipe and the breather pipe are degreased and cleaned as a pretreatment for brazing, and brazing is conducted by using BAg-4 (Low-temperature brazing material) at a temperature of 750-850° C. Removing of the flux and cleaning are conducted as a post-treatment for brazing, and finally coating is conducted.
申请公布号 US6810573(B2) 申请公布日期 2004.11.02
申请号 US20030408419 申请日期 2003.04.07
申请人 BESTEX KYOEI CO., LTD. 发明人 MORINAGA MIKIO;KASHIMA HIROSHI;NAKAMURA TAKASHI;TADA MINORU;HIRAKAWA SHINJI
分类号 F02M37/00;B21D37/18;B21D41/02;B21D53/88;B23K1/00;B23K1/20;B23K31/02;B23K35/30;B23P15/00;B60K15/04;C22C5/06;(IPC1-7):B23P25/00 主分类号 F02M37/00
代理机构 代理人
主权项
地址