摘要 |
A process for producing a low-profile, high-strength dilatation catheter balloon is disclosed. The process comprises forming a tubular extrudate and quenching said extrudate in a cryogenic fluid. The quenched extrudate has morphology of a largely disordered material. The crystallinity in the extrudate is no more than 15%. The crystallinity of the extrudate is measured using X-ray crystallography or DSC. The extrudate is further processed in a mold in which the extrudate is longitudinally and radially stretched. The stretched extrudate is finally attached as a balloon to the distal end of a catheter.
|