摘要 |
<p><P>PROBLEM TO BE SOLVED: To obtain a polyethylene-based resin for a blow molded product, having high density and excellent impact resistance/full notch creep characteristics; and to provide the blow molded product comprising the resin. <P>SOLUTION: The polyethylene-based resin composition has 3.0-10.0 g/10 min melt flow rate (at 190°C under 21.6 kg load), 940-967 kg/m<SP>3</SP>density and >35 nm long-range order obtained by X-ray diffraction of a pressed sheet. The blow molded product is obtained by using the resin composition. <P>COPYRIGHT: (C)2005,JPO&NCIPI</p> |