摘要 |
PROBLEM TO BE SOLVED: To provide a resin composition excellent in antistatic performance, transparency, impact resistance and rigidity, and a molded article of which surface intrinsic resistance value is 10<SP>10</SP>-10<SP>12</SP>Ω, obtained by molding the resin composition. SOLUTION: This resin composition excellent in the balance of physical properties and transparency, and having a continued antistatic performance as compared with conventional antistatic resin is obtained by adding a polyesteramide to a specific rubber-modified styrenic resin, and the molded article is obtained by molding the resin composition. COPYRIGHT: (C)2005,JPO&NCIPI
|