发明名称 INNER WEAR PRODUCED BY USING POLYAMIDE FIBER
摘要 PROBLEM TO BE SOLVED: To provide inner wear excellent in opacity and light shielding properties by making titanium oxide uniformly scatter, exerting refreshing feeling such as dryness, cool feeling or dry feeling, and excellent in color development more than that of conventional one even though the cross-sectional surface of a fiber is not formed into an irregular shape without using compound fiber lacking in versatility where the girth or the number of filaments is not easily changed because of its expensive cost. SOLUTION: The polyamide fiber contains 3.0-6.5 % of titanium oxide and 0.01-1.0 % of a magnesium compound, and has 4.0×10<SP>-5</SP>-8.0×10<SP>-5</SP>mol/g. The polyamide fiber has the following structure: the titanium oxide is uniformly dispersed on the inside part and the surface of the polyamide fiber; a single yarn fiber of the polyamide fiber is 0.5-3.0 dtex; Young's modulus is 20-40 cN/dtex; and the coefficient of dynamic friction between yarns (μ) is 0.15-0.5. The inner wear is produced by using such polyamide fiber. COPYRIGHT: (C)2005,JPO&NCIPI
申请公布号 JP2004292982(A) 申请公布日期 2004.10.21
申请号 JP20030086778 申请日期 2003.03.27
申请人 TORAY IND INC 发明人 MORIOKA KANAME;WATANABE KENSUKE;SUZUKI AKIRA
分类号 A41B17/00;D01F6/90;(IPC1-7):A41B17/00 主分类号 A41B17/00
代理机构 代理人
主权项
地址