发明名称 METHOD FOR MANUFACTURING ROOM TEMPERATURE-CURABLE POLYORGANOSILOXANE COMPOSITION
摘要 PROBLEM TO BE SOLVED: To obtain a room temperature-curable polyorganosiloxane composition exhibiting excellent properties after cured and having a reduced tack-free time. SOLUTION: This room temperature-curable polyorganosiloxane composition comprises (A) a polyorganosiloxane having at both ends a trialkoxy group and obtained by condensing a silanol group-terminated polyorganosiloxane with a tetraalkoxysilane in an excess molar amount based on the amount of the silanol group in the polyorganosiloxane, (B) a silica powder having a specific surface area of at least 50 m<SP>2</SP>/g, (C) a specific organosilane or a partial hydrolyzate thereof, and (D) a titanium chelate catalyst. The method for manufacturing the room temperature-curable polyorganosiloxane composition comprises controlling the amount of the tetraalkoxysilane to at most 0.5 wt% of the component (A) by pressure reduction and/or heating when mixing the component (A) with the component (B), and subsequently adding the components (C) and (D). COPYRIGHT: (C)2004,JPO&NCIPI
申请公布号 JP2004269817(A) 申请公布日期 2004.09.30
申请号 JP20030066195 申请日期 2003.03.12
申请人 GE TOSHIBA SILICONES CO LTD 发明人 IIDA ISAO
分类号 C08L83/04;C08K3/36;(IPC1-7):C08L83/04 主分类号 C08L83/04
代理机构 代理人
主权项
地址