摘要 |
PROBLEM TO BE SOLVED: To obtain a polyacetal resin composition and its molded article from which release of formaldehyde is reduced by improving thermal stability of a polyacetal resin itself at the mixing/kneading, molding, or the like. SOLUTION: This polyacetal resin composition is obtained by incorporating 0.01-10 pts.wt. of an aromatic amine-based compound (B) of a specified structure to 100 pts.wt. of the polyacetal resin (A). COPYRIGHT: (C)2004,JPO&NCIPI
|