摘要 |
<P>PROBLEM TO BE SOLVED: To provide a manufacturing method of an organic electroluminescent device with uniform and reduced thickness, capable of sealing an organic EL element without including bubbles. <P>SOLUTION: At first, a plurality of organic EL elements 50 are formed on a substrate 1. Next, a sealing agent 11 is formed on a lower surface (a color filter 21 side) of outer peripheral part of a sealing plate 20, then a sealing agent 10 is dripped at a central part of the sealing plate 20. After that, the sealing plate 20 and the substrate 1 are stuck with a prescribed pressure in a vacuum chamber in a vacuum state and the vacuum state in the vacuum chamber is released. The base plate 1 and the sealing plate 20 are taken out from the vacuum chamber, and the sealing agents 10, 11 between the substrate 1 and the sealing plate 20 are cured by a curing method for respective materials. <P>COPYRIGHT: (C)2004,JPO&NCIPI |