摘要 |
PROBLEM TO BE SOLVED: To provide an automobile interior and exterior parts comprising a thermoplastic resin composition having flexibility, excellent layer peel-off resistance and excellent painting property. SOLUTION: The automobile interior and exterior parts are formed by melting and kneading (A) and (B) and comprise a thermoplastic resin composition in which a weight ratio of (A) and (B) is 98/2-50/50. (A): styrene-acrylonitrile copolymer, (B): methyl methacrylate-butadiene-styrene copolymer. The styrene-acrylonitrile copolymer is a copolymer in which a repeating unit derived from styrene and a repeating unit derived from acrylonitrile are copolymerized at random. The content of acrylonitrile is usually 2-50 wt.% making the whole of the styrene-acrylonitrile copolymer as 100 wt.%, preferably 20-30 wt.%. COPYRIGHT: (C)2004,JPO&NCIPI
|