摘要 |
PROBLEM TO BE SOLVED: To improve the recycling rate of a generated soil in manufacturing a soil mortar. SOLUTION: In this method, the generated soil is dried by a dryer and ground/finely granulated to such a particle size that a particle with a maximum particle diameter can be conveyed by an air vehicle. Next, a solidifying material is added/mixed and then the generated soil mixed with the solidifying material is conveyed to a kneading water mixing site by the air vehicle. At the kneading water mixing site, the kneading water is mixed to manufacture the soil mortar. COPYRIGHT: (C)2004,JPO&NCIPI
|