摘要 PROBLEM TO BE SOLVED: To solve the problem that polarization resistance acquired by the linear polarization resistance method has often contained environmental resistance in its resistance value. SOLUTION: A potential sweep is performed at a potential of approximately±10 mV with respect to the natural potential of a reinforcing bar at a speed, which indicates an environmental resistance (at which the potential is swept very fast), and a potential sweep is performed at a speed, which indicates the sum of the polarization resistance and the environmental resistance (at which the potential is swept very slowly). On the basis of the difference between the acquired sum of the polarization resistance and the environmental resistance and the acquired environmental resistance, the polarization resistance is determined to compute a corrosion current density. COPYRIGHT: (C)2004,JPO&NCIPI
申请公布号 JP2004226135(A) 申请公布日期 2004.08.12
申请号 JP20030011803 申请日期 2003.01.21
申请人 PORT & AIRPORT RESEARCH INSTITUTE;SHO BOND CONSTR CO LTD 发明人 HAMADA HIDENORI;YAMAJI TORU;HIRASAKI TOSHIFUMI;KOMURE KENICHI
分类号 G01N27/26;(IPC1-7):G01N27/26 主分类号 G01N27/26
代理机构 代理人
主权项
地址