摘要 |
A method of forming a continuous composite structure includes the steps of predetermining relative proportions of a liquid resin forming material, a catalyst, and a inhibitor from respective reservoir (32, 33, 34) based on the ambient temperature and a porous blanket. The predetermined proportions are recirculated independently substantially continuously and coordinated at preselected rates. The predetermined proportions are simultaneously withdrawn and continuously mixed in a chamber (39) having a dispensing outlet (40). A pool (46) of the mixture is formed on the blanket (44) and a leading edge (68) is advanced substantially immediately into permanent contact with a preselected final surface and adhered thereto. Part of the catalyzed and inhibited resin forming material migrates through the blanket to form a continuous resin matrix therein.
|