发明名称 CORROSION RESISTANT ALLOY WITH LITTLE THERMAL EXPANSION
摘要 PROBLEM TO BE SOLVED: To provide a corrosion resistant alloy with little thermal expansion, which has a mean coefficient of heat expansion between 30°C and 200°C controlled low in order to have the coefficient of heat expansion matched to other members in a range between an approximately atmospheric temperature and a warm temperature, and has superior corrosion resistance as well. SOLUTION: The corrosion resistant alloy with little thermal expansion comprises, by mass%, 0.15% or less C, 8.5% or more but less than 10.0% Cr, exceeding 56.0% but less than 58.0% Co, and the balance substantially Fe. The corrosion resistant alloy preferably comprises, by mass%, 0.01-0.15% C, 9.0% or more but less than 9.5% Cr, exceeding 56.5% but 57.0% or less Co and the balance substantially Fe, and has a mean coefficient of heat expansion of 4.0×10<SP>-6</SP>/°C to 7.0×10<SP>-6</SP>/°C between 30°C and 200°C. The alloy also preferably includes, by mass%, 0.005% or more but less than 0.5% S. COPYRIGHT: (C)2004,JPO&NCIPI
申请公布号 JP2004204255(A) 申请公布日期 2004.07.22
申请号 JP20020371964 申请日期 2002.12.24
申请人 HITACHI METALS LTD 发明人 NISHIDA JUNICHI
分类号 C22C19/07;(IPC1-7):C22C19/07 主分类号 C22C19/07
代理机构 代理人
主权项
地址