摘要 |
The composite conductor plate of a low-temperature fuel cell poses the following problem: it must be extremely corrosion-resistant to pure oxygen that is humidified by water and to pure hydrogen and must at the same time be able to be processed mechanically. To solve the problem, a composite conductor plate contains 50 to 60 wt. % Ni, 12 to 22 wt. % Cr, 10 to 18 wt. % Mo, 4 to 10 wt. % Fe and 0.5 to 5 wt. % W. |