摘要 |
The present invention relates to a method for joining two or more components and/or construction parts, at least one of which consists of a dispersion-strengthened alloy having the following composition (in % by weight): C up to 0.08 Si up to 0.7 Cr 10-25 Al 1-10 Mo 1.5-5 Mn up to 0.4 balance Fe as well as normally occurring impurities by the fact that the cross section in the joint is enlarged by forging before joining and where the product manufactured according to the method can be used in high-temperature applications at temperatures above 900° C. |