摘要 |
Polytetrahydrofuran, polytetrahydrofuran copolymers, diesters or monoesters of these polymers are prepared by polymerization of tetrahydrofuran in the presence of at least one telogen and/or comonomer, which is in the form of shaped catalyst bodies or catalyst particles having a volume of the individual shape of the body or particle of at least 0.05 mm<SUP>3</SUP>, preferably at least 0.2 mm<SUP>3</SUP>, in particular 1 mm<SUP>3</SUP>, and has at least one of the features a) and b): a) a pore radius distribution having at least one maximum in the pore radius range from 100 to 5000 Å, b) a pore volume of catalyst pores having radii of 200-3000 Å of greater than 0.05 cm<SUP>3</SUP>/g and/or a pore volume of pores having radii of 200-5000 Å of greater than 0.075 cm<SUP>3</SUP>/g and/or a pore volume of pores having radii of >200 Å of greater than 0.1 cm<SUP>3</SUP>/g. |