摘要 |
PROBLEM TO BE SOLVED: To provide a decorative coating material capable of forming a natural stone tone-coated film having a dignified feeling and excellent in smoothness by one time coating. SOLUTION: This coating material having 100-2,000 Pas viscosity is constituted by containing 100 pts. wt. binder as a solid portion, 30-1,200 pts. wt. granular aggregate and 1-100 pts. wt. crush resistant scaly aggregate. The mean long diameter of the crush resistant scaly aggregate is desirably 1-10 mm. COPYRIGHT: (C)2004,JPO
|