发明名称 |
СПОСОБ ВОССТАНОВЛЕНИЯ ИЗНОШЕННЫХ ДЕТАЛЕЙ ИЗ АЛЮМИНИЕВЫХ СПЛАВОВ |
摘要 |
FIELD: restoration of worn parts of aluminum alloys, for example restoring and strengthening surfaces (for impellers of water pump) of lids of distributing gear wheels of engines. ^ SUBSTANCE: method for restoring worn parts of aluminum alloys in order to prevent superheating comprises steps of building-up restored surface by soldering at temperature 500 - 520 C while using solder B65 and flux 34w; after mechanical working subjecting part to shot blasting at rate of shot flow 50 - 60 m/s. ^ EFFECT: enhanced physical and mechanical properties, improved corrosion resistance of coating. ^ 1 tbl |
申请公布号 |
RU2002124078(A) |
申请公布日期 |
2004.03.20 |
申请号 |
RU20020124078 |
申请日期 |
2002.09.10 |
申请人 |
Орловский государственный аграрный университет |
发明人 |
Коломейченко Александр Викторович;Титов Николай Владимирович;Чернышов Николай Сергеевич |
分类号 |
B23P6/00 |
主分类号 |
B23P6/00 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|