摘要 |
<p><P>PROBLEM TO BE SOLVED: To provide a conductive recycled molded product having the nearly same conductivity as the one obtained by using only virgin pellets even by heightening the proportion of repellets, having hardly reduced properties except the conductivity and having very high practicability. <P>SOLUTION: The conductive recycled molded product having k3 (10<SP>4</SP>≤k3≤10<SP>7</SP>)Ωsurface resistivity lower than k1 is obtained by mixing repellets (A) obtained by melting, kneading, cooling and granulating a used molded product obtained by molding a polyphenylene ether-based resin composition, and having k1 (10<SP>6</SP>≤k1≤10<SP>11</SP>)Ωsurface resistivity, with virgin pellets (B) comprising at least one kind of a polyphenylene ether-based resin and having k2 (10<SP>2</SP>≤k2≤10<SP>6</SP>)Ωsurface resistivity in a weight ratio of (5/95)-(90/10), and molding the mixed resin. <P>COPYRIGHT: (C)2004,JPO</p> |