发明名称 |
PRODUCTION METHOD OF BELT FOR STAINLESS STEEL CONTINUOUSLY VARIABLE TRANSMISSION BELT |
摘要 |
<p>When a metastable austenitic stainless steel strip with a value Md(N), which is calculated from a composition, of 20-100 is ring-rolled to a steel belt, the relationship of -0.3913T+0.5650Md(N)+60.46 epsilon ≥ 65.87 is established among a material temperature T, an equivalent strain epsilon and the value Md(N). Due to the controlled rolling, a stainless steel belt for a continuously variable transmission is bestowed with fatigue properties similar or superior to those of a 18%-Ni maraging steel belt. The value Md(N) is defined by the equation of Md(N)=580-520C-2Si-16Mn-16Cr-23Ni-300N-10Mo, and the equivalent strain epsilon is defined by the equation of epsilon = <SQRT>4(ln(1 - R))<2> /3</SQRT> (R: reduction). Furthermore, the steel belt is stabilized in its quality and profile by confining a variation DELTA T of the material temperature T within a range of +/-6.4 DEG C. <IMAGE></p> |
申请公布号 |
EP1380358(A1) |
申请公布日期 |
2004.01.14 |
申请号 |
EP20020708636 |
申请日期 |
2002.03.22 |
申请人 |
NISSHIN STEEL CO., LTD. |
发明人 |
NISHIO, KATSUHIDE,;SAKAKI, MASAHITO,;UMAKOSHI, YOSHIYUKI,;HARA, KENJI,;TOMIMURA, KOUKI, |
分类号 |
B21B37/74;B21B3/02;B21B5/00;B21B45/00;(IPC1-7):B21B5/00 |
主分类号 |
B21B37/74 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|