发明名称 METHOD FOR PREVENTING HARDNESS VARIATION OF HOT-ROLLED COIL
摘要 PROBLEM TO BE SOLVED: To provide a method that prevents periodic hardness variation generated at the end of a hot-rolled coil and that reduces thickness deviation caused in a cold-rolled steel plate. SOLUTION: A coil car 2 that transports a hot-rolled coil 1 wound at 400-700°C to a placing table is heated at 80°C or above in the contact part 4 with the hot-rolled coil 1, thereby suppressing martensitic transformation caused by locally cooled outer circumferential part of the hot-rolled coil. In addition, it is even more desirable that the coil placing table is also heated or insulated in the contact part with the hot-rolled coil or that the hot-rolled coil placed on the coil placing table is covered with a heat-retaining cover. COPYRIGHT: (C)2004,JPO
申请公布号 JP2004001019(A) 申请公布日期 2004.01.08
申请号 JP20020157678 申请日期 2002.05.30
申请人 NIPPON STEEL CORP 发明人 KATSURA NAOYUKI;ITAZURI YASUHIRO;DOI HIROYUKI;HISHINUMA NORIYUKI
分类号 B21B39/00;B21B45/00;B21C47/24;(IPC1-7):B21B45/00 主分类号 B21B39/00
代理机构 代理人
主权项
地址