发明名称 |
Production of dry, starch-based substance for use as binder in paper production involves mixing a starch-based component, e.g. rye flour, with water in an extruder at elevated temperature and then drying and milling the extrudate |
摘要 |
A granular to powdery, starch-based substance is obtained by mixing a starch-containing component with water in an extruder at 120-250 (preferably 160-220) degreesC with a total water content of less than 40 (preferably 15-20) wt% in the mixture and then drying, milling and sieving the extruded product. A method for the production of a granular to powdery starch-containing mixture by mixing a starch-containing component (A) in an extruder with a water-containing component (B), in which (a) the total water content of the mixture of (A) and (B) is less than 40 (preferably 15-20) wt%, (b) the temperature during mixing and heating is 120-250 (preferably 160-220) degreesC, (c) the extruded product is dried and (d) the dried extrudate is milled and sieved. An Independent claim is also included for a mixture made by this method.
|
申请公布号 |
DE10224355(A1) |
申请公布日期 |
2003.12.11 |
申请号 |
DE20021024355 |
申请日期 |
2002.05.29 |
申请人 |
BUEHLER AG, UZWIL |
发明人 |
BRUEMMER, THOMAS |
分类号 |
C08B30/14;C08L3/00;C08L99/00;C09J199/00;D21H17/28;(IPC1-7):C09D103/02;C08B30/06;C08J3/12;C09D5/12 |
主分类号 |
C08B30/14 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|