摘要 |
A nickel-chromium-molybdenum alloy that is thermally stable and resistant to wet process phosphoric acid and chloride induced localized attack contains in weight percent 31.0 to 34.5% chromium, 7.0 to 10.0% molybdenum, up to 0.2% nitrogen, up to 3.0% iron, up to 1.0% manganese, up to 0.4% aluminum, up to 0.75% silicon, up to 0.1% carbon with the balance nickel plus impurities. |