摘要 |
PROBLEM TO BE SOLVED: To provide an aromatic polycarbonate resin composition excellent in flame retardance, resistances to impact, heat, and wet heat, and melt stability. SOLUTION: This resin composition contains (A) 100 pts.wt. aromatic polycarbonate resin of which the ratio of phenolic terminal groups to the total terminal groups is 5-70 mol%, (B) 0-40 pts.wt. thermoplastic resin other than an aromatic polycarbonate resin, (C) 0.01-1 pt.wt. inorganic compound particles, (D) 0.001-0.5 pt.wt. at least one metal salt selected from among alkali and alkaline earth metal salts, and (E) 0.01-1 pt.wt. fluoropolymer. COPYRIGHT: (C)2004,JPO
|