摘要 |
PROBLEM TO BE SOLVED: To develop a polyethylene terephthalate resin composition improved in mechanical strengths and having moldability, dimensional stability, appearance properties, heat resistance, and weathering resistance. SOLUTION: The polyethylene terephthalate resin composition is prepared by compounding 100 pts.mass (A) polyethylene terephthalate resin with 20-150 pts.mass (B) reinforcement and 0.1-5 pts.mass (C) epoxy group-containing substance. Desirably, the epoxy group-containing substance C comprises one or more of resins selected from among glycidyl ether epoxy resins and glycidylamine epoxy resins. COPYRIGHT: (C)2004,JPO
|