发明名称 ATMOSPHERIC PRESSURE LEACH PROCESS FOR LATERITIC NICKEL ORE
摘要 An atmospheric leach process in the recovery of nickel and cobalt from lateritic ores, said processing including the steps of: a) separating the lateritic ore into a low magnesium containing ore fraction, and a high magnesium containing ore fraction by selective mining or post mining classification; b) separately slurrying the separated ore fractions; c) leaching the low magnesium containing ore fraction with concentrated sulphur ic acid as a primary leach step; and d) introducing the high magnesium content ore slurry following substantial completion of the primary leach step and precipitating iron as goethite or another low sulphate containing form of ir on oxide or iron hydroxide, wherein sulphuric acid released during iron precipitation is used to leach the high magnesium ore fraction as a secondar y leach step.
申请公布号 CA2484134(A1) 申请公布日期 2003.11.13
申请号 CA20032484134 申请日期 2003.03.14
申请人 QNI TECHNOLOGY PTY LTD 发明人 BARNETT, STEVEN;LEWIS, CORALIE ADELE;NEUDORF, DAVID;GILLASPIE, JAMES D.;LIU, HOUYUAN
分类号 C22B23/00;C22B3/04;C22B3/08;C22B3/44;(IPC1-7):C22B23/00 主分类号 C22B23/00
代理机构 代理人
主权项
地址