摘要 |
<P>PROBLEM TO BE SOLVED: To provide a coating composition which can form a cured film excellent in scratch resistance and adhesion to an antireflection film, to provide an optical member excellent in scratch resistance and little in deterioration in the adhesion of the cured film to the antireflection film, and to provide a method for producing the optical member. <P>SOLUTION: The coating composition is one which forms a cured film interposed between a plastic substrate and an antireflection film comprising an inorganic oxide and contains an organosilicon compound and an adhesion improver comprising an acetylene compound having a specified structure. <P>COPYRIGHT: (C)2004,JPO |