摘要 |
The present invention refers to a method of making a Belleville spring comprising the steps of mechanically coiling a flat strip (S) of hardened spring steel into a continuous, generally flat circular convolution (C), said coiled strip (S) having first and second parallel edges (150, 152) defining a width (w), said coiled convolution (C) of said spring steel strip (S) having a given radius of curvature and an axially extending center of generation where said first edge (150) has a first formed radius and said second edge (152) has a second formed radius, with said first radius being less than said second radius by an amount generally equal to said width (w) of said strip, cutting said coiled spring steel strip (S) of said circular convolution (C) to create a generally flat ring shaped spring (B) with first and second free ends (20, 210, 22, 212, 310, 312) joining said free ends (20, 210, 22, 212, 310, 312). In order to create a method of making a Belleville spring with a reduced scrap production and with avoiding deleterious effects of edge imperfections the method is characterized by the step of heating said flat ring shaped spring (B) on a temperature of over 426,7 DEG C (800 DEG F) and simultaneously forming said flat ring shaped spring (B) under axial pressure to heat set said ring shaped spring (B) into a frusto-conical shape. <IMAGE> |