摘要 <p>PROBLEM TO BE SOLVED: To obtain a deoxidizing resin composition excellent in processing stability, scarcely emitting a malodor and slightly deteriorating a polyolefin which is a constituent material with time. SOLUTION: This deoxidizing resin composition comprises 10-80 wt.% of a deoxidizer, 20-90 wt.% of a polyolefin and 10-20,000 ppm of at least one antioxidant selected from the group consisting of a phenolic antioxidant, a phosphorus- based antioxidant and a lactonic antioxidant. The antioxidant is a mixture of at least one antioxidant selected from the group consisting of the phosphorus- based antioxidant and the lactonic antioxidant with the phenolic antioxidant. The content of the antioxidant is 100-20,000 ppm and the deoxidizer is a deoxidizer containing a reducing substance causing an oxygen absorbing reaction by receiving the feed of moisture as a principal ingredient. Thereby, the deterioration of the polyolefin resin is suppressed at the time of thermal processing and preserving and the emission of a malodor and the deterioration of strength are prevented.</p>
申请公布号 JP3460801(B2) 申请公布日期 2003.10.27
申请号 JP19990014544 申请日期 1999.01.22
申请人 发明人
分类号 A23L3/00;A23L3/3436;B01J20/26;B01J20/28;B32B7/02;B32B27/18;B32B27/32;B65D81/26;C08K3/08;C08K3/16;C08K5/10;C08K5/13;C08K5/49;C08L23/00;(IPC1-7):B32B7/02;A23L3/343 主分类号 A23L3/00
代理机构 代理人
主权项
地址