发明名称 METHOD OF PREPARATION OF LIGHT-WEIGHT GROUTING MORTAR
摘要 FIELD: well construction. SUBSTANCE: method includes mixing of oil-well Portland cement with aluminosilicate microspheres and subsequent introduction into produced dry mix of mixing fluid containing cement setting accelerator and water, and their mixing. Mixing of oil-well Portland cement and aluminosilicate microspheres is effected in weight ratio of (80:90)-(10:20). Mixing fluid additionally contains oxyethylcellulose or hydrooxyethylcellulose and lignosulfonates or reagent based on melanine with the following their relation to weight of said dry mix, wt.p.p.: cement setting accelerator 0.2-3.0; oxyethylcellulose or hydrooxyethylcellulose 0.3-0.5; lignosulfonate or reagent based on melanine 0.1- 0.4; water 44-50. After introduction of mixing fluid, mixing is carried out for 0.5h. EFFECT: provided imparting to prepared mortar of high sedimentation stability, good pumpability, lower filtrate loss, controlled terms of setting and time of thickening, higher strength to cement stone with thickening, higher strength to cement stone with improved adhesion properties and low permeability. 2 tbl
申请公布号 RU2215124(C1) 申请公布日期 2003.10.27
申请号 RU20020103679 申请日期 2002.02.08
申请人 OBSHCHESTVO S OGRANICHENNOJ OTVETSTVENNOST'JU "PER;MNIPINEFT 发明人 TATAUROV V.G.;CHUGAEVA O.A.;KUZNETSOVA O.G.;FEFELOV JU.V.;AKULOV B.A.;ZUEVA N.A.;SAZHINA E.M.
分类号 C09K8/473;E21B33/138;(IPC1-7):E21B33/138 主分类号 C09K8/473
代理机构 代理人
主权项
地址