发明名称 |
Sulfoaluminous clinker without iron and without free lime, its process of preparation and its use in white binders |
摘要 |
The lightly colored sulfoaluminous clinker contains: more than 55% by weight of calcium sulfoaluminate phase (C4A3S) more than 10% by weight of belite phase (C2S) less than 10% by weight of anhydrite (CS ) and contains practically no ferrite phase, nor a gehlenite phase (C2AS), nor free lime. It is prepared by a process of roasting carried out at temperatures comprised between about 1250° C. and 1350° C. It can be used for a wide range of applications by combining it with a source of calcium sulfate and/or Portland cement, to obtain binders having specific properties (color, setup time, mechanical strength, expansion or contraction . . . ).
|
申请公布号 |
US2003183131(A1) |
申请公布日期 |
2003.10.02 |
申请号 |
US20020278836 |
申请日期 |
2002.10.24 |
申请人 |
CLASSEN BRUNO;COLOMBET PIERRE |
发明人 |
CLASSEN BRUNO;COLOMBET PIERRE |
分类号 |
C04B7/32;C04B28/06;(IPC1-7):C04B7/48;C04B7/36 |
主分类号 |
C04B7/32 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|