摘要 |
PROBLEM TO BE SOLVED: To provide a polyoxymethylene resin composition so excellent in thermal stability that it can stand a high temperature and long time molding. SOLUTION: To the polyoxymethylene resin composition, a metal salt of a saturated fatty acid, 0.001-5 pts.wt. at least a compound selected from the group consisting of an alkali metal inorganic compound, and then an alkaline earth metal inorganic compound is added to 100 pts.wt. polyoxymethylene resin and then, 0.001-5 pts.wt. metal salt of a saturated fatty acid is added. COPYRIGHT: (C)2003,JPO
|