发明名称 NON-HEAT-TREATED STEEL
摘要 PROBLEM TO BE SOLVED: To provide non-heat-treated steel which, even when the heating temperature in hot rolling fluctuates, can prevent the dispersion of hardness, thus securing stable mechanical properties. SOLUTION: This non-heat-treated steel comprises 0.35-0.55% C, 0.10-2.0% Si, 0.5-1.6% Mn, 0.10-0.25% S, 0.001-0.05% Al, 0.05-0.30% Ti, 0.0080% or lower N, and the balance being Fe and impurities, has a value of Ti (%)-3×S (%) lower than -0.1, and, if necessary, may further contain at least one of Ca, Mg, and Te and/or at least one of V, Cr, and Ni. COPYRIGHT: (C)2003,JPO
申请公布号 JP2003268487(A) 申请公布日期 2003.09.25
申请号 JP20020068757 申请日期 2002.03.13
申请人 SUMITOMO METAL IND LTD 发明人 TAIRA HIROAKI
分类号 C22C38/00;C22C38/14;C22C38/60;(IPC1-7):C22C38/00 主分类号 C22C38/00