发明名称 METHOD FOR RECOVERING VALUABLE METAL FROM SCRAP OF LAMINATED CERAMIC CAPACITOR
摘要 <p><P>PROBLEM TO BE SOLVED: To provide a method for recovering valuable metals such as nickel in high purity, by easily separating a binding material from scrap of laminated ceramic capacitors. <P>SOLUTION: This recovering method comprises crushing scrap of the laminated ceramic capacitors into pieces, leaching nickel into sulfuric acid, neutralizing the obtained post-leaching liquid in a range of pH 1-5, to precipitate the dissolved binding material, separating it, neutralizing the post-leaching liquid after the binding material has been precipitated and separated, in the range of pH 6-9 to precipitate nickel, separating the post-leaching liquid in which the binding material remains, and dissolving the obtained precipitates again in sulfuric acid to obtain a nickel solution. <P>COPYRIGHT: (C)2003,JPO</p>
申请公布号 JP2003268459(A) 申请公布日期 2003.09.25
申请号 JP20020062887 申请日期 2002.03.08
申请人 SUMITOMO METAL MINING CO LTD 发明人 FUKUI ATSUSHI;IMAMURA MASAKI
分类号 C22B7/00;C22B3/04;C22B3/44;C22B23/00;(IPC1-7):C22B7/00 主分类号 C22B7/00
代理机构 代理人
主权项
地址
您可能感兴趣的专利