发明名称 CHEMICALLY TOUGHENED GLASS
摘要 <p>PCT No. PCT/FR93/01035 Sec. 371 Date Sep. 29, 1995 Sec. 102(e) Date Sep. 29, 1995 PCT Filed Oct. 21, 1993 PCT Pub. No. WO94/08910 PCT Pub. Date Apr. 28, 1994This invention has as its subject a panel, preferably produced by the float process, reinforced by surface ion exchange for a long period at a temperature such that the exchanged depth is greater than 250 microns for surface compressive stresses exceeding 400 MPa, and greater than 75 microns for surface compresive stresses exceeding 700 Mpa, and the matrix of which complies with one of the following compositions, expressed in percentages by weight: SiO2:65 to 76% Al203:1.5 to 5% MgO:4 to 8% CaO:0 to 4.5% Na2:10 to 18% K2O:1 to 7.5% B2O3:0 to 4% these elements representing at least 96% of the weight of the glass and complying, in addition, with the percentages by weight 0<CaO/CaO+MgO<0.45 and 0.05<K2O/Na2O+K2O<0.35.</p>
申请公布号 EP0665822(B2) 申请公布日期 2003.09.24
申请号 EP19930924101 申请日期 1993.10.21
申请人 SAINT-GOBAIN GLASS FRANCE 发明人 CHARRUE, HERVE;GUILLEMET, CLAUDE;CREPET, RENEE;RIFQI, FRANCOISE
分类号 C03C3/085;C03C3/087;C03C3/091;C03C21/00;(IPC1-7):C03C3/085 主分类号 C03C3/085
代理机构 代理人
主权项
地址