摘要 |
<p>An impermeable sintered ceramic electrolyte layer of a solid oxide fuel cell is formed by depositing ceramic powder on a substrate using electrophoretic deposition, isostatically pressing that deposited ceramic layer and then heating the compressed ceramic powder layer at temperatures below 1000 °C. In preferred embodiments the ceramic thick film fuel cell assembly is formed upon a ferritic stainless steel substrate.</p> |