摘要 |
In the method, a long nip (N) shoe calender formed of a shoe roll (10) and a thermo roll (20) is used. In calendering, a nip dwell time which is over 10 ms. advantageously over 20 ms. a nip pressure which is below 3 MPa. advantageously below 1 MPa. and a surface temperature of the thermo roll (20) which is over 200° C. advantageously over 250° C. are used. In addition, the board web (W) surface to be pressed against the thermo roll (20) is moisturized before the nip.
|