<p>The alloys comprises (wt. %): Cr 2-24, Mn 7-14, Si 3-8, the balance being Ni. Opt. 0.05-4.0% Mo and 0.05-1.0% B are added. The alloy is cast into a glass test tube and drawn with it to form an insulated microwire. The microwires have stable chemical composition and electrical properties (relatively high resistance and low thermal coefficient thereof).</p>
申请公布号
DE1946394(A1)
申请公布日期
1971.03.18
申请号
DE19691946394
申请日期
1969.09.12
申请人
AFONINA,LJUDMILA G.;KALOSIN,NIKOLAJ P.;FIRSOW,ANATOLIJ M.;ALFTAN,ERMININGELD;DEJANOWA,SWETLANA W.;KARASIK,NAUM J.
发明人
G. AFONINA,LJUDMILA;P. KALOSIN,NIKOLAJ;M. FIRSOW,ANATOLIJ;ALFTAN,ERMININGELD;W. DEJANOWA,SWETLANA;J. KARASIK,NAUM