发明名称 |
OPERATING METHOD IN SLAG-MAKING STAGE IN COPPER CONVERTER |
摘要 |
PROBLEM TO BE SOLVED: To provide a method for operating a copper converter by which a copper grade in a matte supplied into the copper converter is enhanced to 64-68% without deteriorating slag characteristic and the production capacity of a copper smelting furnace can be improved. SOLUTION: A heat quantity to be get out with nitrogen is reduced by increasing a blasting oxygen concentration to 29.5-32.0% for 64-68% copper grade in the matte and the blowing oxygen amount can be reduced until reaching to 1300°C mainly with FeS oxidizing reaction heat, and the slag characteristic is not deteriorated. COPYRIGHT: (C)2003,JPO
|
申请公布号 |
JP2003193144(A) |
申请公布日期 |
2003.07.09 |
申请号 |
JP20010391594 |
申请日期 |
2001.12.25 |
申请人 |
NIPPON MINING & METALS CO LTD |
发明人 |
NAGATO TOSHIHIRO |
分类号 |
C22B15/06;(IPC1-7):C22B15/06 |
主分类号 |
C22B15/06 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|