发明名称 METHOD FOR BLASTING CALIBRATION OF CHILL MOLD
摘要 PROBLEM TO BE SOLVED: To provide a method for blasting calibration of a chill mold including a tubular mold or a block mold in a relatively simple manner and at a relatively small cost. SOLUTION: In a method for blasting calibration of the chill mold, a calibrating mandrel is inserted into the chill mold 1, an explosive material is placed on an outer surface 4 of the chill mold 1, and ignited. The inner side 3 of the chill mold 1 is pressed against the calibrating mandrel by the explosive force, and brought to the setpoint measure. In a mold wall 2, the chill mold 1 has bores 5 for cooling means and for measuring elements, which extend in the longitudinal direction LR of the chill mold 1, and exit at end faces 6 and 7 of the mold wall 2. Before the blasting calibration, the bores 5 are filled up with a free-flowing material and tightly closed. The free-flowing material is preferably an incompressible fluid and/or a built material. COPYRIGHT: (C)2003,JPO
申请公布号 JP2003191053(A) 申请公布日期 2003.07.08
申请号 JP20020344044 申请日期 2002.11.27
申请人 KM EUROP METAL AG 发明人 HAURI ROLAND
分类号 B22C9/12;B21D3/00;B21D3/14;B21D26/08;B22D7/06;B22D11/057;(IPC1-7):B22D11/057 主分类号 B22C9/12
代理机构 代理人
主权项
地址