摘要 |
The present invention provides a method for producing an ethylene-vinyl acetate copolymer (EVA) containing 5 mol% to 60 mol% of ethylene, by copolymerizing ethylene and vinyl acetate with a polymerization initiator, in which an aliphatic alcohol having not more than four carbon atoms is used as the polymerization solvent, the contents of acetaldehyde and a saturated acetic ester with respect to vinyl acetate are not more than 200 ppm, and 10 ppm to 1500 ppm, respectively, and polymerization is carried out at a temperature of 30 DEG C to 150 DEG C. EVA obtained by the foregoing method may be saponified to obtain a saponified ethylene-vinyl acetate copolymer (EVOH). According to the present invention, at least one of (i) improved melt-extrusion stability, (ii) improved melt-moldability, (iii) reduced discoloration, and (iv) reduced gelation is achieved. |