摘要 |
PROBLEM TO BE SOLVED: To obtain a reinforced polyamide resin composition excellent in electroconductivity, and good in heat stability, impact resistance, and surface appearance of a molded article. SOLUTION: This reinforced thermoplastic resin composition is manufacture by adding (B) 3-50 pts.wt. of an agent for providing electroconductivity, and (C) 5-50 pts.wt. of a reinforcing member, to (A) 100 pts.wt. of a thermoplastic resin composition comprising (a) 85-50 wt.% of a polyamide resin, (b) 10-45 wt.% of a composite rubber comprising a polyorganosiloxane rubber component and a polyalkyl (meth)acrylate rubber component, and (c) 5-40 wt.% of an impact resistance improving agent. This composition is used for manufacturing a molded article. COPYRIGHT: (C)2003,JPO
|