发明名称 Slenderized animal fiber and method for preparation thereof
摘要 A slenderized crimped animal fiber with a fixed slenderized form having a lowering rate of tensile strength for undyed spun yarn of no less than 10%, fiber contraction in boiling water of no more than 1%, an alkali solubility of no more than 22% by weight and a UB solubility of no more than 35% by weight, wherein the slenderized crimped animal fiber is prepared by being drawn by practically 1.20 to 1.60 times after an anisotropic swelling is given to the animal fiber consisting of bilateral structure using swelling plasticization with base.
申请公布号 US2003068493(A1) 申请公布日期 2003.04.10
申请号 US20010950587 申请日期 2001.09.13
申请人 UMEHARA RYO;KANDA TAKASHI;YAMADA MASARU;KARAKAWA TADASHI 发明人 UMEHARA RYO;KANDA TAKASHI;YAMADA MASARU;KARAKAWA TADASHI
分类号 D02G1/00;D06M11/50;D06M11/54;D06M11/76;D06M11/84;D06M13/368;D06M23/00;(IPC1-7):D02G3/00 主分类号 D02G1/00
代理机构 代理人
主权项
地址