The antifouling composition of the present invention includes a glassy matrix formed by crosslinking a mixture of a silanol-terminated silicone and an alkoxy-functionalized siloxane to provide an interpenetrating polymer network of glass and silicone and at least two materials capable of microphase separation, at least one of which is graftable to the glassy matrix. A primer composition is also provided and is a mixture of an epoxy, an alkoxy-functionalized siloxane and a silane capable of compatabilizing the epoxy and the alkoxy-functionalized siloxane; a glassy matrix formed by crosslinking a mixture of a silanol-terminated silicone and an alkoxy-functionalized siloxane.